| Typical Properties | Test Method | Test Condition | GF10 Value |
GF20 Value |
GF30 Value |
Unit |
| Density | DIN EN ISO 1183 | 23℃ | 1.26 | 1.31 | 1.4 | g/cm³ |
| Shrinkage | GB 15585 | 0.6-0.9 | 0.4~0.6 | 0.2~0.4 | % | |
| Tensile Strength | DIN EN ISO 527 | 50mm/min | 80 | 125 | 138 | MPa |
| Tensile Modulus | DIN EN ISO 527 | 50mm/min | 5000 | 6800 | 9700 | MPa |
| Elongation at Break | DIN EN ISO 527 | 50mm/min | 2.5 | 2.3 | 2 | % |
| Flexural Strength | DIN EN ISO 178 | 2mm/min | 125 | 150 | 180 | MPa |
| Flexural Modulus | DIN EN ISO 178 | 2mm/min | 3800 | 5700 | 7100 | MPa |
| Izod Notched Impact Strength | DIN EN ISO 180 | 4mm,23℃ | 7.5 | 9 | 12.3 | KJ/M² |
| Izod Unnotched Impact Strength |
DIN EN ISO 180 | 4mm,23℃ | 48 | 65 | 80 | KJ/M² |
| Flame retardant properties | UL94 | 0.75mm | V1 | V1 | V1 | |
| Flame retardant properties | UL94 | 1mm | V0 | V0 | V0 | |
| Flame retardant properties | UL94 | 1.5mm | V0 | V0 | V0 | |
| Flame retardant properties | UL94 | 3mm | V0/5AV | V0/5AV | VO/5AV |