| Product Description | ||||
| Resin Identification | 30% carbon fiber reinforced; superior to CF20 in strength, stiffness, wear resistance, dimensional stability, and heat resistance. | |||
| Color | Black | |||
| Main applications | High-strength robotic joint arms Premium bicycle frames, racing ski bindings Aerospace and defense Drone airframes High-temperature engine components | |||
| Processing Method | Injection Molding | |||
| Typical Properties | Test Method | Test Condition | Value | Unit |
| Physical Properties | ||||
| Density | DIN EN ISO 1183 | 23℃ | 1.4 | g/cm³ |
| Melt Flow Rate | DIN EN ISO 1133 | 400℃/5kg | 50 | g/10min |
| Shrinkage | GB 15585 | 0.3-0.5 | % | |
| Mechanical Properties | ||||
| Tensile Strength | DIN EN ISO 527 | 50mm/min | 265 | MPa |
| Tensile modulus | 28000 | MPa | ||
| Elongation at Break | 1.7 | % | ||
| Flexural Strength | DIN EN ISO 178 | 2mm/min | 280 | MPa |
| Flexural Modulus | 24000 | MPa | ||
| Cantilever Beam Unnotched Impact Strength |
DIN EN ISO 180 | 4mm,22℃ | 50 | KJ/M2 |
| Izod Notched Impact Strength | DIN EN ISO 180 | 4mm,23℃ | 7.3 | KJ/M2 |
| Thermal Performance | ||||
| Heat Deformation Temperature | DIN EN ISO 75 | 1.8MPa Unannealed | 315 | ℃ |
| Heat Deformation Temperature | DIN EN ISO 75 | 0.45MPa Unannealed | 330 | ℃ |
| Melting temperature | DIN EN ISO 11357 | 340 | ℃ | |
| linear expansion coefficient | DIN EN ISO 11359 | Flow, below Tg | 5.00E+00 | μm/m/℃ |
| linear expansion coefficient | DIN EN ISO 11359 | Flow, above Tg | 6.00E+00 | μm/m/℃ |
| Thermal Performance | ||||
| Surface Resistance | IEC 60093 | 23℃ | 1.00E+03 | Ω.CM |
| Volume Resistance | IEC 60093 | 23℃ | 1.00E+03 | Ω.CM |
| insulation strength | IEC 60243 | 2.0mm | 25 | KV/mm |
| dielectric strength | IEC 62631-2-1 | 23℃ 1 KHz | 17 | |
| dissipation factor | IEC 62631-2-1 | 23℃ 1 MHz | 0.023 | |
| CTI | IEC 60112 | 150 | V | |
| Flame retardant properties | ||||
| Flame retardant properties | UL94 | 0.3mm | V0 | |
| Flame retardant properties | UL94 | 0.5mm | V0 | |
| Flame retardant properties | UL94 | 1mm | V0 | |
| Flame retardant properties | UL94 | 1.5mm | V0 | |
| Glow wire flammability index | IEC60695-2-12 | 0.75mm | 850 | ℃ |
| Glow wire flammability index | IEC60695-2-12 | 1.5mm | 850 | ℃ |
| Glow wire flammability index | IEC60695-2-12 | 3mm | 960 | ℃ |
| Glow wire flammability index | IEC60695-2-13 | 0.75mm | 850 | ℃ |
| Glow wire flammability index | IEC60695-2-13 | 1.5mm | 850 | ℃ |
| Glow wire flammability index | IEC60695-2-13 | 3mm | 960 | ℃ |
Note:
(1) Data represents typical values and is provided solely as a reference for customer use. It does not constitute a guarantee of minimum or maximum quality standards or any other purpose.
(2) Performance may vary across different colors.
Caution:
The data and information in this document are based on our current knowledge and experience. Should new knowledge or experience emerge in the future, we reserve the right to modify the information and data herein without prior notice. As usage conditions and applicable laws may vary by location and time, customers are responsible for determining whether the products and information herein are suitable for their specific applications. Customers must ensure their workplaces and product handling methods comply with applicable laws and other governmental regulations. Lixin New Materials assumes no liability or obligation regarding the information in this document and makes no warranties. All implied warranties of merchantability or fitness for a particular purpose are hereby expressly excluded.
| Typical Injection Molding Process | ||||
| Plastic Drying | ||||
| Drying Time | 2~4h | |||
| Drying Temperature | 130~150℃ | |||
| Drying Equipment | Hot-air dryer | |||
| Drying Type | Continuous drying (production process) | |||
| Injection Molding Process | ||||
| Nozzle Section | 370~390℃ | |||
| Plastics Section | 380~400℃ | |||
| Conveying Section | 360~380℃ | |||
| Maximum Injection Temperature | 450℃ | |||
| Injection Pressure | 30~70MPa | |||
| Injection Speed | 30~75mm/s | |||
| Plasticization Pressure Velocity | Pressure: 35–70 MPa Speed: 50–100 mm/s | |||
| Plasticization Back Pressure | 20~60MPa | |||
| Recommended Mold Temperature | 170~220℃ | |||
Disclaimer: The above injection molding processes may vary depending on product geometry, mold design, injection molding machine specifications, and other factors. Specific adjustments should be made based on actual conditions.